Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX7110 - Americas - (PPE+PP) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX7110 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 10.6 g/10min ASTM D 1238
온도 260 °C -
하중 5 kg -
기계적 특성단위시험규격
ASTM 데이터
인장탄성률 1340 MPa ASTM D 638
항복강도 35 MPa ASTM D 638
파단시 강도 32 MPa ASTM D 638
항복변형률 6.5 % ASTM D 638
파단시 신율 195 % ASTM D 638
굴곡 계수 1550 MPa ASTM D 790
아이조드 충격은 노치, 1/8 in 437 J/m ASTM D 256
아이조드 충격은 노치, Low-Temperature 149 J/m ASTM D 256
온도 -30 °C -
열적 특성단위시험규격
ISO 데이터
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 1.0 mm -
ASTM 데이터
DTUL @ 66 psi 113 °C ASTM D 648
DTUL @ 264 psi 77 °C ASTM D 648
비카트 연화 온도 138 °C ASTM D 1525
기타 특성단위시험규격
밀도 970 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 60 - 65 °C -
Pre-drying - Time 2 - 4 h -
Processing humidity ≤0.02 % -
용융수지온도 260 - 290 °C -
성형온도 30 - 50 °C -
Zone 1 225 - 275 °C -
Zone 2 240 - 280 °C -
Zone 3 250 - 290 °C -
Screw speed 20 - 100 rpm -
Back pressure 0.3 - 0.7 MPa -
특징
생산 공정
사출 성형, 시트 압출
응용
자동차의
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.